Weld Joint Factor (AS4041 Table 3.12.2) Class Design Factor (AS4041 Table 3.12.3) Material Design Strength, MPa (AS4041, Appendix D) Pipe Outside Diameter from Pipe Charts, mm Nominal Wall Thickness from Pipe Charts, mm Manufacturing Tolerance ( %) Corrosion Allowance, mm Depth of Threading, Grooving or Machining, mm Design Wall Thickness, mm Maximum Allowable Operating Pressure, MPa e M f D t nom 0.85 0.70 130 26.9 3.2 10.0 1.0 0.0 1.88 13.68 Product of e x M not less than 0.7 e xM 0.7

Manufacturing Tolerances Aust Pipes 10%; American Pipes

tf MAOP

oduct of e x M not less than 0.7

anufacturing Tolerances ust Pipes 10%; American Pipes 12.5%