Aluminium plate (thickness= 100 mm, width= 5000 mm, melting point = 660 0C) is rolled at room temperature to achieve the
thickness of 85 mm. Diameter of rolled used is 1 m with the coefficient of friction is 0.2.
a. Calculate the maximum possible draft of the process. [3 MARKS]
b. Is it possible to do a single rolling from 100 to 85 mm? Why? [1 MARK]
c. Calculate the force required (N) to do rolling process if the average true stress is 250 MPa. [2 MARKS]
d. If the process is done at 3000C, determine whether it is cold rolling or hot rolling. [2 MARKS]
e. Compare the microstructure formed by rolling at room temperature and at 3000C. [2 MARKS]
Answer: