2. Perparing the materials photoresist blue paint & diluent, the diluent can be
replaced by banana oil (blue paint : diluent = 1 : 3).
4. Paint the copper clad laminate by diluted photoresist blue paint and spread
it in one derection evenly.
10. The distance between the lamp and the glass is about 10cm.
11. Preparing to develop. (20g photoresist dry film developer mixes with
800ml 30 water)
12. Put the plate into the develop solution and brush it gently.
17. Preparing the materials of etching. (200g etching powder mixes with
800ml 100 water)
18. Begin to etching. Put the plate into the etching solution. The temperature
of the solution had better in 50 above.
19. Preparing the materials of remove. (50g photoresist resist remover powder
mixes with 1000ml water)