BARAKO TIE-IN 5CR PIPE WELDING PMI RESULT = LOW ALLOY

Prior Start of welding, QC/Supervisor ensures that the correct rod/filler shall be used
by conducting PMI. When the PMI result is satisfactory, welding will commence.
Moreover during welding, QC is conducting spot inspection of rod/filler by checking
the rod/filler package on site.