fr Aluminium
Welding filler metals
for aluminium
EN ISO 18273
AWS A5.10 DIN 1725 EN 573/753/1706 %
Union AlMg 4.5 Mn Zr AlMg 4.5 Mn 3.3547 EN AW-5083 [AlMg 4.5 Mn 0.7] Al Rest / Balanced
S Al 5087 (AlMg4.5MnZr) AlMg 4 Mn 3.3545 EN AW-5086 [AlMg 4] Mn 0.7 - 1.1
ER5087 AlMg 5 3.3555 EN AW-5019 [AlMg 5] Cr 0.05 - 0.25
AlMgSi 0.5 3.3206 EN AW-6060 [AlMgSi] Mg 4.5 - 5.2
AlMgSi 0.7 3.3210 EN AW-6005A [AlSiMg(A)] Zr 0.1 - 0.2
AlMgSi 1 3.2315 EN AW-6082 [AlSi 1 MgMn] Ti <0.15
AlMg 1 SiCu 3.3211 EN AW-6061 [AlMg 1 SiCu] Fe <0.4
AlZn 4.5 Mg 1 3.4335 EN AW-7020 [AlZn 4.5 Mg 1] Si <0.25
G-AlMg 5 3.3561 EN AC-51300 Zn <0.25
G-AlMg 5 Si 3.3261 EN AC-51400
Union AlMg 4.5 Mn AlMg 4.5 Mn 3.3547 EN AW-5083 [AlMg 4.5 Mn 0.7] Al Rest / Balanced
S Al 5183 (AlMg4.5Mn0.7(A)) AlMg 4 Mn 3.3545 EN AW-5086 [AlMg 4] Mn 0.5 - 1.0
ER5183 AlMg 5 3.3555 EN AW-5019 [AlMg 5] Cr 0.05 - 0.25
AlMgSi 0.5 3.3206 EN AW-6060 [AlMgSi] Mg 4.3 - 5.2
AlMgSi 0.7 3.3210 EN AW-6005A [AlSiMg(A)] Ti <0.15
AlMgSi 1 3.2315 EN AW-6082 [AlSi 1 MgMn] Si <0.4
AlMg 1 SiCu 3.3211 EN AW-6061 [AlMg 1 SiCu] Zn <0.25
AlZn 4.5 Mg 3.4335 EN AW-7020 [AlZn 4.5 Mg 1] Cu <0.1
G-AlMg 5 3.3561 EN AC-51300
G-AlMg 5 Si 3.3261 EN AC-51400
Rp0.2 125 MPa 1.0 2.0 DB (61.132.04) DB (61.132.04) EN ISO 14175: EN ISO 14175:
Rm 275 MPa 1.2 2.4 WIWEB GL I1 I1, I3
A (L0=5d0) 17% 1.6 3.2 WIWEB
Rp0.2 125 MPa 1.0 1.6 TV (2196) TV (2195) EN ISO 14175: EN ISO 14175:
Rm 275 MPa 1.2 2.0 DB (61.132.03) DB (61.132.03) I1 I1, I3
A (L0=5d0) 17% 1.6 2.4 WIWEB GL
3.2 LR
4.0 DNV
WIWEB
BV
Rp0.2 110 MPa 1.0 1.6 TV (2198) TV (2197) EN ISO 14175: EN ISO 14175:
Rm 240 MPa 1.2 2.0 DB (61.132.01) DB (61.132.01) I1 I1, I3
A (L0=5d0) 17% 1.6 2.4 GL
3.2 LR
Rp0.2 40 MPa 1.0 1.6 DB (61.132.02) DB (61.132.02) EN ISO 14175: EN ISO 14175:
Rm 120 MPa 1.2 2.0 I1 I1, I3
A (L0=5d0) 8% 1.6 2.4
3.2
4.0
Is a pure aluminium welding wire for joining and surfacing of aluminium materials according to EN ISO 18273.
It is a welding consumable with Ti for grain refinement and weldable in all positions.
Schweistbe und Drahtelektroden zum WIG- und MIG-Schweien von AlMg-Legierungen bis 3% Mg. Das Schweigut ist seewasserbestndig.
Fr annhernd farbgleiche Schweiverbindungen an anodisch oxidierbaren Werkstoffen. Werkstckflanken grndlich reinigen.
Dicke Bleche auf 150C vorwrmen.
Solid wires and rods for GTAW and GMAW of AlMg alloys containing up to 3% Mg. Seawater resistant weld metal. Good colour matching with
base metal after anodizing. Thorough cleaning of the workpiece bevels is necessary. Thicker plate materials require preheating to 150C (302F).
Zirkon-mikrolegierte Schweistbe und Drahtelektroden. Das Schweigut ist heirissunempfindlich. Besonders vorteilhaft bei komplizierten
Schweikonstruktionen mit ungnstigen Einspannverhltnissen. Werkstckflanken grndlich reinigen. Dicke Bleche auf 150C vorwrmen.
Zirconium micro alloyed welding rods and bare wire electrodes. The weld metal is not susceptible to hot cracking.
Particularly advantageous for complicated weldments involving damp conditions.
Thorough cleaning of the workpiece bevels is necessary. Thicker plate materials require preheating to 150C (302F).
Schweistbe und Drahtelektroden zum WIG- und MIG-Schweien von AlMg-Legierungen. Das Schweigut ist seewasserbestndig.
Werkstckflanken grndlich reinigen. Dicke Bleche auf 150C vorwrmen.
Solid wires and rods for GTAW and GMAW of AlMg alloys. Seawater resistant weld metal.
Thorough cleaning of the workpiece bevels is necessary. Thicker plate materials require preheating to 150C (302F).
Schweistbe und Drahtelektroden zum WIG- und MIG-Schweien von AlMg-Legierungen bis 5% Mg.
Das Schweigut ist seewasserbestndig.
Werkstckflanken grndlich reinigen. Dicke Bleche auf 150C vorwrmen.
Solid wires and rods for GTAW and GMAW of AlMg alloys containing up to 5% Mg.
Seawater resistant weld metal. Good colour matching with base metal after anodizing.
Thorough cleaning of the workpiece bevels is necessary. Thicker plate materials require preheating to 150C (302F).
Schweistbe und Drahtelektroden zum WIG- und MIG-Schweien. Gasschweien bzw. Hartlten mit geeigneten Flussmitteln mglich.
Das Schweigut ist nicht dekorativ anodisch oxydierbar. Sehr flssiges Schweibad. Dicke Bleche und Gusstcke auf 150 - 200C vorwrmen.
Die Schweinhte an Werkstcken aus aushrtbaren Legierungen in nicht hchstbeanspruchte Zonen legen.
Solid wires and rods for GTAW and GMAW. Oxyacetylene welding respectively brazing with suitable fluxes possible.
The weld metal is not suitable for anodizing for decorative purposes. Very fluid weld pool. Thicker plate materials and castings require
preheating to 150 - 200C (302 - 392F). Do not use for welding hardenable alloys is high stressed zones.
Solid wires and rods for GTAW and GMAW of AlMg alloys.
Mg-content max. 3% to obtain intergranular corrosion resistance.
Seawater resistant weld metal. For obtaining near matching coloured joints where anodizing is required.
Die Angaben zur Art und Anwendung unserer Produkte The specifications in regard to the type and application
dienen lediglich der Information des Anwenders. Die of our products are only for the users information. The
Daten zu den mechanischen Eigenschaften beziehen sich data specified for the mechanical properties always
immer auf das reine Schweigut unter Beachtung der refer to the weld metal alone under observance of the
geltenden Normen. In der Schweiverbindung werden die applicable standards. In the weld joint, the weld metal
Schweiguteigenschaften u.a. vom Grundwerkstoff, der properties are influenced, among other factors, by the
Schweiposition und den Schweiparametern beeinflusst. parent metal, the welding position and the welding
Eine Garantie fr die Eignung fr eine bestimmte Art der parameters. A guarantee of suitability for a certain type
Anwendung erfordert in jedem einzelnen Fall eine aus- of application requires an explicit written agreement in
drckliche schriftliche Vereinbarung. each individual case.
Bhler Welding
Global Brand Management
bohler.welding@voestalpine.com
www.boehler-welding.com