Valley Rubber Mixing, a wholly owned subsidiary of

Glo-Mold, Inc., is a supplier of custom-mixed rubber


compounds and calendered goods.
Custom Mixing Calendering Laboratory Research and Development
Valley Rubber Mixing has the flexibility of mixing your Valley Rubber Mixing also has custom calendering Along with calendering our mixed compounds, Valley Rubber Mixing maintains a full-scale
compounds with our open mills or with one of our capabilities. Our 48 variable we can also reprocess your leftover trim, computerized laboratory for formula development,
two internal mixers for larger volume runs. speed, three roll vertical which will help compound scale-up, quality checks on incoming raw
calender, equipped reduce or materials, and outbound customer shipments.
We have a dedicated black line and with chilled eliminate
a separate dedicated color line water take-off waste. Compounds are routinely developed for
where we mix all polymers equipment, ASTM call-outs, military specification,
except silicone. provides Give Valley or per specific customer requests.
exceptional Rubber We also work with several of
By mixing on the open mill, we Mixing a our raw material suppliers when
are able to give you compounds dimensional
control in both call for any exact color match of a compound
with optimum dispersion, better of your is necessary.
physicals and better heat control. width and
gauge. calendering
This also gives us the ability to match needs. As a small to medium size custom
the batch size to the customers needs. mixer, we look forward to working
with our customers in developing new
We can provide mixed compounds for compounds or improving existing
virtually any application from our extensive compounds. Our lab staff can supply
recipe files or will mix to customers recipes you with trial batches from 2 10 lbs.
and specifications.
If you have that labor intensive job, a
To be more competitive on large orders, compound that others dont like to mix
Valley Rubber also mixes with internal mixers. or if you arent satisfied with your current
We have a #3 Farrell (130 lbs.) on our black line supplier, give Valley Rubber Mixing a call.
and a #4 Kobe Side Dump (180 lbs.) on our color line.

Small batch or large run, make Valley Rubber Mixing


your compound source.

520 South Main Street Suite 2445 Akron, Ohio 44311-1010


330-434-4442 valleyrubber.com
Glo-Mold is the unique, Glo-Mold Product
patented rubber compound Selection and Curing
for IN PLACE mold cleaning. Guide for all Polymers

Eliminates or reduces typical problems How Glo-Mold works.


At 275 degrees fahrenheit (135 celsius) , the cure time for RED Glo-Mold will be 20 minutes
and hidden costs of conventional mold
Initial cleaning of very dirty molds may require
cleaning techniques. At 300 degrees fahrenheit (148 celsius), the cure time for RED Glo-Mold will be 17 minutes
multiple applications.
Glo-Mold Advantages
Maintenance of clean molds will be accomplished At 325 degrees fahrenheit (162 celsius), the cure time for RED Glo-Mold will be 15 minutes
Minimize press downtime through determination of optimal number of production
Minimize excessive labor in heats between applications of Glo-Mold. At 340 degrees fahrenheit (171 celsius), the cure time for RED Glo-Mold will be 14 minutes
mold handling
A variety of products allows the fabricator to select At 345 degrees fahrenheit (174 celsius), the cure time for YELLOW Glo-Mold will be 13 minutes
Reduce mold damage or abrasion
the Glo-Mold formulation that best suits the physical,
Reduce delays due to scheduling At 350 degrees fahrenheit (177 celsius), the cure time for YELLOW Glo-Mold will be 12 minutes
rheological and processing requirements.
of cleaning equipment
At 365 degrees fahrenheit (185 celsius), the cure time for YELLOW Glo-Mold will be 11 minutes
Does Glo-Mold work? Reduce number of rejects due to Processing recommendations depending on
defects or poor surface appearance product selection and application. At 380 degrees fahrenheit (193 celsius), the cure time for YELLOW Glo-Mold will be 8 minutes
Over 500 molders worldwide now use Glo-Mold! Reduce heat transfer loss Time: 2 to 20 minutes
At 385 degrees fahrenheit (196 celsius), the cure time for ORANGE Glo-Mold will be 5 minutes
Temperature: 280O F to 450O F
What can Glo-Mold do for you? Normal processing techniques are used
with Glo-Mold in injection, compression and Pressure: Maximum available At 410 degrees fahrenheit (210 celsius), the cure time for ORANGE Glo-Mold will be 3 minutes
No downtime for cleaning. Injecting Glo-Mold through the screw transfer molding.
Mold storage can be accomplished using Glo-Mold At 425 degrees fahrenheit (218 celsius), the cure time for ORANGE Glo-Mold will be 2 minutes
on a regular basis eliminates the need for equipment shutdown.
Preventative maintenance can be extremely as the last heat in a production run. Remove the
effective when Glo-Mold is used regularly. At 450 degrees fahrenheit (232 celsius), the cure time for ORANGE Glo-Mold will be 1 minute
It is possible to spot-clean molds during the production cycle mold in the closed position. The rust inhibitor that is
Molds are kept clean. Costs are reduced. generated by the Glo-Mold will protect for a minimum
when a defect shows up due to localized build-up of dirt. Productivity can be increased 5 10%. GREEN: High hot tear strength - Follow the cure times for Yellow Glo-Mold
of six months. The mold will also be clean when
Eliminate the need for major cleaning equipment associated Cleaning by diffusion is accomplished by returned to production. BLUE: Low mooney - Follow the cure times for Yellow Glo-Mold
with mold handling equipment and valuable floor space for each. penetration of the reactive ingredients through
Most mold surfaces are efficiently cleaned by LAVENDER: non-curing (for use as a clean-out in extruders)- No cure time
the dirt layer and subsequent absorption onto
Glo-Mold. These include steel, stainless steel,
Glo-Mold has been proven to be a very beneficial production tool the surface of the compound. Diffusion can be
chrome and aluminum. Do not use Glo-Mold with WHITE - Follow the cure times for Yellow Glo-Mold
when scheduled routinely. affected by the nature of the dirt, time,
brass or other exotic surfaces.
temperature and pressure.
Easy steps to cleaner molds
Temperature and pressure are critical to ensure Preparation of Glo-Mold should be the same as
maximum cleaning. While higher temperatures used for the normal compound. Glo-Mold can be Check actual mold temperature
increase the diffusion rate, they also reduce the pre-formed, cold-milled, calendered, extruded Select product based on this chart
cleaning time. Cavity pressure should be or diced.
Insert Glo-Mold in usual fashion
maintained by ensuring adequate charge weight.
Do not bump. Precaution should be taken to avoid skin and eye Do not bump, turn off vacuum
contact. Adequate ventilation should be provided.
At room temperature, Glo-Mold may be handled safely.
At elevated temperatures, toxic effects are unknown. 520 S. Main Street, Suite 2445 Akron, OH 44311