1.O-Ring May be Tear or Fitted 1.Make the Chamfer at body on not Properly Both Spindle and both Spindle and Pivot side As Pivot Side. per Drawing. (15 to 20 deg) 2.O-Ring hardness should 2. O-Ring Fitted With Fluid /Water Coming from less than 70 shore A. Proper lubrication with Lub oil. 1 Spindle side and Pivot side 3.Chemfer should not be 3. O-Ring Hardness Valve Provided as per Drawing Should not be less then 70Shore Reqiurement.(15 to 20 deg.) A.
1. Give the instruction to vendor
1.Rubber Moulding Curing for choose the proper Curing Rubber Moulded with time for moulding & choose time not given . 2 backupring not properly proper mixture for the moulding 2. Rubber compund ratio not bonded. procees . properly choose/mix.
1. Radius do not provide at
outer side of the disc . 2.Outeness should be found both in backup ring moulding and Disc also (S.G iron Disc/S.S Disc). Operating Torque the valve is 3. Thickness of the 1.Provide the radius at ourt side 3 more then rubber in bckupring and body of the disc in size above then requirement/competeter moulding is less then 100mm. 2. Reqiurement. Regularly check the moulding die also check the fixture that can be used to machine the disc. 3. Increse the rubber thickness accoding to the Requirement.
4 Face Groove Ring Damage during moulding and testing