Butt weld
-Tensile test- to determine the ultimate
strength of the weld joint
-bend test- To determine the soundness and
ductility of the weld joint
Fillet weld-To determine the size, contour
and degree of soundness
Stud weld- To determine the acceptability
of stud weld by hammering, bend and
tension test
Mechanical Tests
The type and number of test specimens that shall be
tested to qualify a groove weld procedure are given
in QW-451
Sample preparation shall follow QW-463.
If any test specimen required by QW-451 fails to
meet the applicable acceptance criteria, the test
coupon shall be considered as failed.
BUTT WELD
FILLET WELD